Dear Tahir,
You have to follow the following if
1) New tank construction
code of construction :: API 650 App T = NDE requirement
API 650 App U =Ultrasonic Examination in lieu of Radio graphic exam
2)for Tank Maintenance purpose:
API 653 App F =NDE requirement summery .
Hope it will work for you .
On Sun, Feb 7, 2016 at 8:23 PM, SHANMUGA PERUMAL <gosp75@gmail.com> wrote:
Dear tahir,
Ceramic backing tapes /strips can be used.You will search google.you
will get.Esab,lincoln and other reputed brands also available. contact
them for guidance.
Thanks,
BR,
G.S.PERUMAL.
On 2/7/16, tahir alam <tahiralam007@gmail.com> wrote:
> Dear expert
>
> we have contract to construct storage tank in the refinery.
> Here client is telling us not to put backing strip while annular butt joint
> welding and after welding do radiography of joint and they are telling to
> put ceramic baking material bottom side of annular plate.
>
> pls let me know is it possible to do so.And kindly let me know the name of
> ceramic material and whats the function for this.
>
> *Best Regards*
> *Tahir Alam*
>
> *Planning Engineer*
> *Agam Tank Maintenance Group *Mobile : +(965)5150-1509
>
>
> --------------------------------------------------------------------------------
> Site Office : +(965)2388-3614
> Head Office : +(965) 2398-5381l2
> Fax : +(965) 2398-8312
> P.O.Box : 9390 Ahmadi, 61004 Kuwait
> Email : tahiralam007@gmail.com
> Website : www.agamltd.com
> -------------------------------------------------------------
>
> --
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/CAHWTgoOHqdpEn_SGceWSXoa3U70TVOXtkzcXjX1tVpyZtxyRyg%40mail.gmail.com.
> For more options, visit https://groups.google.com/d/optout.
>
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPFTRWkLyPitHWK4NtTVg4V_uEbXsJO11NR2sr%2BmeyGKd5vhoQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Best Regards
*YAKOOB KHAN *
*YAKOOB KHAN *
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABhShnZgKPw91hd5jt66FJN6XcLBtdbw3KdcRVA8ZegmXPRpiQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment