Wednesday, February 3, 2016

Re: [MW:24223] Re: Painting DFT guage for individual layer reading.

Dear All,

No, We can measure the DFT after completion of Final layer also.

In SSPC we have an Instument named TOOKE GAGE or PIG GAGE, it will measure the DFT in each layer, but its a Destructive method. 

You have to do the touch painting after the inspection.
 
Thanks & Best Regards, 
Sujin. J
Sr. Inspection Engineer 
Bureau Veritas.




From: 'prem_nautiyal26' via Materials & Welding <materials-welding@googlegroups.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Wednesday, February 3, 2016 10:20 AM
Subject: Re: [MW:24219] Re: Painting DFT guage for individual layer reading.

After final painting you can only measure the final paint DFT. 
If you needed DFT after primer and first coat then you should have checked earlier.

Regards

Prem Nautiyal



Sent from Samsung Mobile


-------- Original message --------
From: Dinesh Somwanshi
Date:03/02/2016 11:31 AM (GMT+05:30)
To: materials-welding
Subject: Re: [MW:24218] Re: Painting DFT guage for individual layer reading.

Dear ,
 
 I want indivisual reading of primer , intercoat & final reading of DFT for applied paint systems.
 
Regards
 
dinesh

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER
AUTHORIZED WELDING / NDT / PAINTING INSPECTION PERSONNEL,
AWS - CWI , CSWIP 3.1
BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
00919881344135

असो द्यावी दया तुमच्या लागतसे पाया.

Pray for others, sometime, You might never need to pray for yourself again.....

On Wed, Feb 3, 2016 at 10:45 AM, Mohd Siraj <mohd52100@gmail.com> wrote:
question not clear.

you mean by type of DFT gauge to be used for layers?


On Wednesday, February 3, 2016 at 7:20:08 AM UTC+3, dinesh AWS-CWI ,CSWIP 3.1,NDT II wrote:
Dear WI / PI,s,
 
Please provide details of available Painting Guage to define individual paint layer DFT for multi layer paint system.
 
 
DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER
AUTHORIZED WELDING / NDT / PAINTING INSPECTION PERSONNEL,
AWS - CWI , CSWIP 3.1
BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT

असो द्यावी दया तुमच्या लागतसे पाया.

Pray for others, sometime, You might never need to pray for yourself again.....
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/43d65839-106c-429a-a94f-6b1331f6716b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrVPRD1PiQfCKcT1d-DPiZecvK6W1W34Cgx%2B7fS-KdbPqg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/oji2btf2s8j9e7xiqix69v7e.1454480436427%40email.android.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...