Re: [MW:24212] Hardness Of P-91 Material

preheat & PWHT should be carried out based on the approved WPS. chart of preheat & PWHT should be in a continuous chart. 


On Tuesday, February 2, 2016 1:39 PM, elias jarjoura <elias-jarjoura@hotmail.com> wrote:


Pre-heat and PWHT as per approved or adopted PQR and WPS.
 


Date: Sat, 30 Jan 2016 09:59:36 +0500
Subject: [MW:24187] Hardness Of P-91 Material
From: pradipsil@gmail.com
To: materials-welding@googlegroups.com

Dear Everybody,

Some of our P-91 Joints( Weldment) are coming hardness value around 300HB in the HRSG Unit.
 Joints thickness is 18 mm & 20 mm & we did PWHT 2 hours holding time at 710 degree centrigrade also we did 150 degree heating rate ,120 degree cooling rate.

Can you pls suggest us this hardness value  is acceptable in the HRSG unit. If not pls suggest me how to recover.
Regards,
Kumar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8mJXj9twE50bbG4-%2Bb-_35XPHeuAZ97xUD5n1Aq7TR21Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/DUB113-W68C6F01FE06F372AB188708ADF0%40phx.gbl.

For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...