Sunday, February 7, 2016

[MW:24239] Re: Tanks PWHT

you are talking about the clean out door PWHT.

you can proceed the first ,second,third...with vertical joint first and horizontal after ward.

On Friday, January 8, 2016 at 5:31:26 AM UTC+3, Ahmed Sedeek wrote:
 
Dear Members,
 
We have crude and petroleum tanks in which 1 course of shell plates PWHT has to be carried out, so our subcontractor erect and install first , second and third course shell plate I asked if we could start welding in the second course and complete tanks shell without welding vertical and horizontal of the first course, and I want some document from code to approve this method if correct.
 
Regards,

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/703d865b-9790-4e1e-ba63-262b490692f2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...