reason for do so is graphite lining on spiral lining gasket has perfect contact with CS raised face.
-- if cost permit you can use.
On Saturday, February 6, 2016 at 7:23:46 AM UTC+3, Meghanadh K wrote:
On Saturday, February 6, 2016 at 7:23:46 AM UTC+3, Meghanadh K wrote:
Can we use SS spiral wound gasket(316L-inner Ring) for the both CS connecting flanges, I am working in a petrochemical where all the spiral wound gaskets used were SS.Do any code specifies the use spiral wound gasket to particular materials or is it a choice of owner/user.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3ff82703-1e01-4aa0-b267-04a739637f1c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment