[MW:24234] ss spiral wound gasket to cs flanges

Can we use SS spiral wound gasket(316L-inner Ring) for the both CS connecting flanges, I am working in a petrochemical where all the spiral wound gaskets used were SS.Do any code specifies the use spiral wound gasket to particular materials or is it a choice of owner/user.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/def915ef-a7fe-4dfc-a1d6-c4b1d29dd395%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...