Yes this is the only solution to measure the individual layer DFT. After completion of Final coat.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/255516423.1726661.1454644841601.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
This one i had already suggested in 03 Feb 2016.
Thanks and Regards
Sujin.J
Sent from Yahoo Mail for iPhone
-- Sent from Yahoo Mail for iPhone
On Friday, February 5, 2016, 07:50, HIREMATH <hiremath.qaqc@gmail.com> wrote:
Hi,Hope this may help you.
Regards,ANANDSent from my iPhone 5S--Hi,You cannot measure the DFT of each under coat layer once top coat is applied.Let us consider a surface is painted with three coat paint system, A-Primer, B-Mid-coat & C-Topcoat. So thickness can be measured as follows.DFT of Coat 'A' - Can be directly measured once it is applied & dried.DFT of coat 'B' - Actual DFT measured from the surface - DFT of Coat 'A'DFT of coat 'C' - Actual DFT measured from the surface - (DFT of Coat 'A'+DFT of coat 'B')Regards,Lalu RajendranOn Wed, Feb 3, 2016 at 8:18 AM, Dinesh Somwanshi <som.din@gmail.com> wrote:--Dear WI / PI,s,Please provide details of available Painting Guage to define individual paint layer DFT for multi layer paint system.DINESH VITTHAL SOMWANSHIBACHELOR IN MECHANICAL ENGINEERAUTHORIZED WELDING / NDT / PAINTING INSPECTION PERSONNEL,AWS - CWI , CSWIP 3.1BGAS Gr 2 / 3NDT II -UT , RT , MT , PT, VTअसो द्यावी दया तुमच्या लागतसे पाया.Pray for others, sometime, You might never need to pray for yourself again.....
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrUcR_yn2wtMsb0HsfBwJAQ-%3DUDeG4JvJ9d7pe-VofjmRA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13u2XF5sxz-sZqTJryoJ83nNppbgCbPkmgNcHBWaVe5Rog%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/255516423.1726661.1454644841601.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.






Comments