Tuesday, October 13, 2015

Re: [MW:23715] Leak test for HSD Fuel Tank

Pl refer UL 142 standard for deisel tanks

Rgds
G.Prakash
Independent Consultant, ASME/ISO/PED
Tel: +9714 2778511 Mob:+97152 979 5678

On Tue, Oct 13, 2015 at 1:57 PM, pras ari <alhanif.pras@gmail.com> wrote:
Dear Sir,

Please advise me about leak test (hydro-test) of HSD Fuel Tank, I have 2 (two) tank with capacity 1400 KL, We will held Leak test but but site condition and around very difficult to get water as much as 2800 kilo liters.
Is any method for substitute leak test? may be NDT or pneumatic test?


Thanks & Regards
Winarko

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMoAFwrSgBgmU-%3DZKEuaK_YigrM5eBnzrYfTHsyrm%2BUvMSuYcg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4q%2BLbw5Yeb9W3Tpp1gJXsVrCTmyaoKFeO-rw2HaCa6ymrQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...