From: Naveen Raj Sent: Τετάρτη, 7 Οκτωβρίου 2015 - 09:21 To: Materials & Welding Reply To: materials-welding@googlegroups.com Subject: [MW:23674] SS to BRASS Welding |
Dear All,
-- Kindly advise me what welding material will be used to joint SS 304 to BRASS.
We used copper soldering method but the SS tube broken after welding..
Thickness of SS is 0.8mm. Pls find the picture...
Thanks in advance....
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7051d20a-a6e8-4e84-afee-5d6cb653692c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment