Hi

You can get the parameters from the technical person of either your welding consumable supplier or machine supplier. 

Regards

Prem Nautiyal



Sent from Samsung Mobile


-------- Original message --------
From: Nazz A
Date:31/08/2015 10:46 AM (GMT+05:30)
To: Materials & Welding
Subject: [MW:23371] Orbital Tug welding in Cu Ni.

Anybody did the Otbital tig welding by Polysoude machine. Now we are using an orbital machine for welding of Cu Ni pipes.

Please tell the good parameters of root welding.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a1a66a53-9722-449e-94e0-bbd494b8d2b7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...