Re: [MW:23369] PWHT requirement for vessel

What is the base/code backup for your reply? Please let us know so that we can read it.

On Sunday, 30 August 2015 12:13:51 UTC+5:30, gerr...@yahoo.com wrote:
In this case, PWHT is not required, provided

1. minimum applied Preheat is 95degC
 2. Size of the Groove weld is less than 13mm

Thanks & Regards
J.Gerald Jayakumar
0091-9344954677


From: Prasad <prs...@gmail.com>
To: Materials & Welding <material...@googlegroups.com>
Sent: Saturday, August 29, 2015 7:13 PM
Subject: [MW:23361] PWHT requirement for vessel

Construction Code ASME Sec. VIII Div. 1 Edn. 2013
Non pressure Part skirt support
of vertical vessel not welded directly to vessel.
MOC IS 2062 P no.1 Group  1
Thk. 40 mm
No special service requirement.

For this case whether PWHT is mandatory?

Regards,
Prasad G.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d725eb3d-aca0-435c-ba4c-feadeba7f303%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/06d099da-c881-47e9-943b-b4294444213f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...