Re: [MW:23344] Process Piping LTCS PQR with Impact test

if impact is there, refer 31.3

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Tue, Aug 25, 2015 at 3:41 PM, SWI <tulasiramus@gmail.com> wrote:
Dear Group,

While qualifying a PQR as per ASME SEC IX for Process piping ASME B31.3, in WPS the thickness limit will be as per ASME SEC IX QW403.6  or we need to refer QW403.6 & ASME B31.3 Table T323.3.1 A-5.


Regards,

TR

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/393c559c-bd97-4891-95cf-5a964561c77c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOfn18apUH-mUwk8%2Bh4_j_Q3EHwT2Vj7z_EWSgCZPAg1Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...