Thursday, August 20, 2015

Re: [MW:23322] AWS D1.1 Table 4.6 , Clause 8, PWHT.

Riaz,

When Impact test is Applicable, this AWS D1.1 requirement is similar to that of ASME Sec.IX.

Production job shall be minimum 80% Time at Temperature of the PQR test coupon. There is no limitation on the maximum range.

That is why most International specifications like ARAMCO lays emphasis on the maximum time keeping hardness value in mind.
 
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677


From: "Ri@z" <riaz.rafeeque@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Thursday, August 20, 2015 3:19 PM
Subject: [MW:23320] AWS D1.1 Table 4.6 , Clause 8, PWHT.



Dear All


Post Weld Heat Treatment
8) A change in the PWHT temperature and/or time ranges. The PQR test shall be
subject to 80% of the aggregate times at temperature(s). The PWHT total
time(s) at temperature(s) may be applied in one heating cycle


As per above clause, duration of the holding time shall not be lower or higher than the PQR test piece PWHT time.

ie., if PQR done at 100 minute PWHT. WPS is approved for 80 to 120 minutes. AM I RIGHT ??

Please advice.

If time is restricted , then corresponding weld metal thickness also be restricted.  i.e, As per minimum holding time table more than 2"thk shaal be minimum 2 hr and addition each 1 "shall be multiplied by 15 minutes. So is it restrict the minimum and max thickness qualified ???

Please advise


Riaz


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1c23e5ca-34bf-48a0-ab58-7e4e483e2f11%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...