Up to 3" tensile test is carried out for longitudinal only bcz in trasvers , you can't make it straight due to heavy thickness sch-160. Also 4" sch-160- go for longitudinal tensile test.

Reagrds,
Mahek shah
Assist. Manager QA/QC
Larsen & Toubro Ltd

On Sat, Aug 15, 2015 at 5:47 PM, Rathnakar M <rathnakar85@gmail.com> wrote:
Is tensile test on Transverse strip specimen possible on NPS 3 & 4 inch Sch 160 ( Material specification SA-106)

Regards,

Rathnakar Gowda
Material Engineer - QSD
BILFAL Heavy Industries Ltd.
P.O.Box 10138,
Jubail Industrial City 31961, K.S.A.
Tel +966 3 3419304 Ext (212)
Fax + 966 3 341 6717

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/870337a1-0aed-4059-abf0-e707ec877512%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BtkXLRjJazo4B8ALWs1LFy4JRmuJsNpYixovdXAzvJwHM%2B7%2Bg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...