Re: [MW:23312] S.A. 2.5 surface profile

only by grit/abrasive blasting, u will get 2.5

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Wed, Aug 19, 2015 at 10:17 AM, Jayesh Panchal <panchal.jayesh61@gmail.com> wrote:
Dear Jasmin,

Alternatively we can do surface roughness by power brush.
You can try on sample surface & compare with comparator.
If it is found nearer  to sa 2.5, then get approval from client.

Jayesh Panchal

On Wed, Aug 19, 2015 at 8:44 AM, 'Bijay' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Do you want only without sand blasting or without any type of blasting. Now a days sand blasting is rarely used bcoz of its environmental issues. If you want you can blast with copper slag or iron grit. 
But it is not possible without blasting.

Sent from Yahoo Mail on Android


From:"Jasim Ahmed" <jasim.kuet.me@gmail.com>
Date:Tue, 18 Aug, 2015 at 12:34 pm
Subject:[MW:23305] S.A. 2.5 surface profile

Dear experts,

I badly need to know - is it possible to create S.A. 2.5 surface profile for joint wrapping without sand blasting?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5e6cfb73-db6b-48b1-8dbe-a7bb3f93f062%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1439954087.46828.YahooMailAndroidMobile%40web181306.mail.ne1.yahoo.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA%2BqLVs6Y8RETYQvfBtLTQcSqmh0v_akgchrKeG4S565iEPMQA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNyMH6HU3mMGzuLmrjQ%3D%3DXFW6pNyC0yoO%3DrOhRVg7wZeA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...