Re: [MW:23304] NPS 8 & less - Tensile testing.

Dear Mr. Rathnakar,

As per Cl. No. 23.1 of SA 106 of ASME Sec. IIA Ed. 2013, on sizes smaller than NPS 8", only longitudinal tensile test shall be used.

Thanks & regards,

C. R. GANDHI 


From: Vairamuthu Ramar <vairamuthu78@hotmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Sunday, August 16, 2015 8:36 AM
Subject: RE: [MW:23303] NPS 8 & less - Tensile testing.

Hi,
 
Yes. Possible. Please go through the attachment.
 
Regards

 

Date: Sat, 15 Aug 2015 05:17:26 -0700
From: rathnakar85@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:23302] NPS 8 & less - Tensile testing.

Is tensile test on Transverse strip specimen possible on NPS 3 & 4 inch Sch 160 ( Material specification SA-106)

Regards,
Rathnakar Gowda
Material Engineer - QSD
BILFAL Heavy Industries Ltd.
P.O.Box 10138,
Jubail Industrial City 31961, K.S.A.
Tel +966 3 3419304 Ext (212)
Fax + 966 3 341 6717


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/870337a1-0aed-4059-abf0-e707ec877512%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/COL128-W506D7EA753A8666DE0E007DC7A0%40phx.gbl.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...