Hi,
 
Yes. Possible. Please go through the attachment.
 
Regards

 

Date: Sat, 15 Aug 2015 05:17:26 -0700
From: rathnakar85@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:23302] NPS 8 & less - Tensile testing.

Is tensile test on Transverse strip specimen possible on NPS 3 & 4 inch Sch 160 ( Material specification SA-106)

Regards,
Rathnakar Gowda
Material Engineer - QSD
BILFAL Heavy Industries Ltd.
P.O.Box 10138,
Jubail Industrial City 31961, K.S.A.
Tel +966 3 3419304 Ext (212)
Fax + 966 3 341 6717


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/870337a1-0aed-4059-abf0-e707ec877512%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...