Yes, you can make different WPS(s) within the range(s) qualified as per already established PQR if the impact test is not applicable.
When impact test is applicable, all the supplimentary variables will become essential variable and you will have limited provisions to make different WPSs.
Hope, your question is answered.
--------------------------------------------
On Thu, 8/13/15, Chetan <patilvicky4@gmail.com> wrote:
Subject: [MW:23293] WPS Supplementary essential variable for Impact
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Thursday, August 13, 2015, 9:52 AM
Dear
sir,
I have PQR for P1 G1 to P1 G2 as per Impact test
requirement G no. is supplementary essential variable.
My question is can I made P1 G1 to P1 G1 & P1 G2 to P1
G2 wps using same PQR without change in other essential
& supplementary variable.
--
You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/55cc30cc.4366460a.c86fb.39ea%40mx.google.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1439467147.60490.YahooMailBasic%40web122402.mail.ne1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment