Thursday, August 13, 2015

Re: [MW:23295] WPS Supplementary essential variable for Impact

Yes, you can use the same PQR for individual combination. However be sure to perform all the mechanical test including charpies on both base metal side P1 G1 and P1 G2.

Regards
Mohankumar K

On Thursday, August 13, 2015, Chetan <patilvicky4@gmail.com> wrote:
Dear sir,

I have PQR for P1 G1 to P1 G2 as per Impact test requirement  G no. is supplementary essential variable.
My question is can I made P1 G1 to P1 G1 & P1 G2 to P1 G2 wps using same PQR without change in other essential & supplementary variable.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/55cc30cc.4366460a.c86fb.39ea%40mx.google.com.
For more options, visit https://groups.google.com/d/optout.


--
Regards
Mohankumar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEQCnx0JwiE31M8jquZqK8Og%3DqzkkDiBWkbkybNbP4L6MHkwYw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...