Re: [MW:23283] RE: 23278] blind welded to pipe at test limit

In b31.3 its mentioned only using blanks and spades  ,not welded blanks.
On 7 Aug 2015 06:52, "Asif Raza" <asif.raza@yascotech.com> wrote:
>
> Dear it is not acceptable at all. Pl ask for the required standard and Specs which is valid as per the B31.1.
>
>  
>
> Peter
>
> Welding Eng.
>
>  
>
> From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Jayasuryan Raveendran
> Sent: Thursday, August 06, 2015 2:36 PM
> To: materials-welding@googlegroups.com
> Subject: [MW:23278] blind welded to pipe at test limit
>
>  
>
> Dear frnds
>
> For hydro test limit contractor does not have any blind flange or end caps so contractor requesting to diectly weld blind to the pipe. Is it acceptable. Any references for that. Constrtion code b31.3 test pressure 44 kgf per cm square
>
> Regards
> Jayasuryan
>
> --
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at http://groups.google.com/group/materials-welding.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGt3MynrnPY%3D3LPhP2tw2s2c_s3tTGb410uvn7o1bbVyCqM75w%40mail.gmail.com.
> For more options, visit https://groups.google.com/d/optout.
>
> --
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at http://groups.google.com/group/materials-welding.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/55c35a77.691db50a.956bf.205aSMTPIN_ADDED_BROKEN%40gmr-mx.google.com.
> For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGt3Mymk-uLYvqjQO3%3D-MfgAF0z_sz4jtSdd-edoq_VJYhw0vA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...