[MW:23333] Re: regarding- thickness range for LTCS piping material for WPS

Dears,
         Good day.I have one doubt about LTCS PQR regarding
temperature limit.Our PQR specimen is 5mm thickness and impact test at
2.5mm thick.In your design
temp.is -46 degree.In ASME 31.3 and section
viii says .this 2.5 mm specimen allowed for -27degree.But our client comment is this PQR IS used only
-28 degree only.So explain about the correct thickness of specimen for
impact test at -46 temp.design temp.

Thanks and Regards


On Thursday, April 19, 2012 at 8:42:35 AM UTC+3, Darshan Maheshwari wrote:
Can any body suggest what thickness range is applied for qualifying a WPS (for thickness 7.11mm) for LTCS piping material. Please provide reference also.
 
Regards,

Darshan Maheshwari.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e1fc4d6c-20c5-4aca-a8ff-802430eae1e4%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...