[MW:23313] Re: Reg:Longitudinal tensile and bend test

Dears,
What should be the limit for "MARKEDLY" difference for the different metals. For instance, 1st parent material ductility is 15%, the other base material is 23%.. than can we consider this difference as a "marked" difference and choose longitudinal bending as per QW 161.5?
Thanks,


23 Nisan 2014 Çarşamba 09:24:35 UTC+3 tarihinde Avinash Pandey yazdı:
Dear All

1. I have a query regarding transverse bend test and longitudinal bend test mention in ASME sec.IX.
2.when to use these test  for procedure qualification.

Regards 
Avinash Pandey

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f90c15b0-6849-454a-b319-bef56ffda1e6%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS