Saturday, August 15, 2015

[MW:23301] difference between ECT, RFET, IRIS, MFL and APR

Hello experts,

I'm currently in search of the advantages and disadvantages of ECT, RFET, IRIS, APR and MFL in heat exchanger tube testing. The info that I need are:

- time taken to complete the inspection per tube
- level of tube cleanliness
- material suitability
- % of equipment error
- type of defects detected and undetected including under baffle
- defect sizing capability

Thanks in advance

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/40c98dc8-844f-42f5-a991-210a2ae799c4%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...