I would say that you have an area of underpenetrated root to the right and a mighty area of over-penetration where the welder has burnt through. It is a clear reject but maybe someone else will do a formal assessment to API 1104 criteria.
Alan Denney
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Subramani, Kulandaivel
Sent: 12 August 2015 20:38
To: materials-welding@googlegroups.com
Subject: [MW:23291] RT Film Intrepretation
Dear Members,
Please find attached image of a RT film taken on a repaired area on a 24" Diameter and WT 12.7mm.
The original welding process were GTAW Root and SMAW fill and Cap.
How can we classify this defect?
The Acceptance standard for this is API 1104.
Please shed some light on this.
Thanks for your support.
Subramani.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/006d01d0d536%2453c1e270%24fb45a750%24%40batelco.com.bh.
For more options, visit https://groups.google.com/d/optout.
This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/001501d0d5c7%248ad3aa00%24a07afe00%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.
Alan Denney
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Subramani, Kulandaivel
Sent: 12 August 2015 20:38
To: materials-welding@googlegroups.com
Subject: [MW:23291] RT Film Intrepretation
Dear Members,
Please find attached image of a RT film taken on a repaired area on a 24" Diameter and WT 12.7mm.
The original welding process were GTAW Root and SMAW fill and Cap.
How can we classify this defect?
The Acceptance standard for this is API 1104.
Please shed some light on this.
Thanks for your support.
Subramani.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/006d01d0d536%2453c1e270%24fb45a750%24%40batelco.com.bh.
For more options, visit https://groups.google.com/d/optout.
This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/001501d0d5c7%248ad3aa00%24a07afe00%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.
Comments