Dear Members,
Please find attached image of a RT film taken on a repaired area on a 24" Diameter and WT 12.7mm.
The original welding process were GTAW Root and SMAW fill and Cap.
How can we classify this defect?
The Acceptance standard for this is API 1104.
Please shed some light on this.
Thanks for your support.
Subramani.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/006d01d0d536%2453c1e270%24fb45a750%24%40batelco.com.bh.
For more options, visit https://groups.google.com/d/optout.
Please find attached image of a RT film taken on a repaired area on a 24" Diameter and WT 12.7mm.
The original welding process were GTAW Root and SMAW fill and Cap.
How can we classify this defect?
The Acceptance standard for this is API 1104.
Please shed some light on this.
Thanks for your support.
Subramani.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/006d01d0d536%2453c1e270%24fb45a750%24%40batelco.com.bh.
For more options, visit https://groups.google.com/d/optout.

Comments