[MW:23291] Do we need to run new PQR for using TIG dressing/wash to correct pipe alignment.

Dear All Expert
Refer to QW 404.14 of ASME Sec IX.
Do we need to run new PQR for using TIG dressing/wash to correct pipe alignment as per ASME B31.3& Sec IX.
In my opinion I think process of TIG dressing should not be subjected to QW 404.14 because it's doesn't join two part together.
I'd appreciate all of your sharing and reference.

Regards

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/86418645-2371-45ad-9677-b4fd12877267%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...