On Mon, Jul 27, 2015 at 5:39 PM, RAJENDRA PRASAD TRIPATHI <rptripathi2000@gmail.com> wrote:
For large Steel structure fabrication , it will be 2.5-3% of steel weight. Only for rough calculation.

Thanks
Vinay Tripathi
+919643886124(India)

On Saturday, May 9, 2015 at 11:57:36 AM UTC+5:30, Neem Lal wrote:
suppose i am going to weld 16 mm thick plate with single v groove butt weld for a length of 1 meter,
then how much kg of weld or electrodes is required?
apart from general triangular rule, is there any thumb rule?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2229b530-a9ee-432e-9d1d-b52f5e5ea14f%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkKqHJrpE0qO0UxOyoUfy8kMF6ndgYLjKmnq1XCHQwYQaA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...