Monday, July 20, 2015

Re: [MW:23177] Pressure testing for in service exchanger

1.5 times. better you do helium leak test to identify any leaks in tubes to baffle welds

On Thu, Jul 9, 2015 at 5:04 PM, Narender Reddy <malgireddy.2010@gmail.com> wrote:
Dear experts

I have problem regarding Pressure testing for in service vessel.
1). As per API 510 pressure test required after any repair or alteration.And as per the code requirements it is 1.5*mawp*stress ratio.But my question is we did not conduct any repair or alteration on the exchanger we want know the any leaks present inside tubes and is there any deference between inspection pressure test(leak identification for the tubes only) and standard pressure test as per design pressure.
2).If there is a difference STD hydro test and leak inspection test for tubes.which type of pressure test we need to conduct to identify the leaks and at what pressure we need conduct.

Best regrds
Narender reddy.M

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c4833219-1cb4-4563-9ed8-1f0e762aa6d5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC-DWSvLhxN7Gf9SWNxWUT6ZOBPtk%3D7cUNmZLdM2GSQtjM9QJg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS