please provide more details regarding application, stream handeled oerating conditions, Dwng. history of joint, etc
ahmed eissa
material and corrosion engineer
--------------------------------------------
On Sun, 7/12/15, Ramesh Bapat <rbapat@hotmail.com> wrote:
Subject: [MW:23152] 20 Chrome/32 Nickel, Nb- Centrifugally cast tubes
To: materials-welding@googlegroups.com
Cc: rbapat@hotmail.com
Date: Sunday, July 12, 2015, 2:22 PM
Hello Experts Client has encountered
what appears to be a corrosive attack in the HAZ of the pipe
to tee welds on Metaltek 20/32 Nb material. This area was
solution annealed at 2000 F for 6 hours. The corroded/eroded
areas were not present prior to solution annealing based on
previous inspection.
The area has been penetrant tested with no
relevant indications. It has also been examined by phased
array with no evidence of cracking. It appears the base
metal has eroded under the weld bead in the area of the
HAZ.
Can you please offer opinions on the cause and
corrective actions, if possible?Thanks and Best
Regards,Ramesh
--
You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BAY403-EAS148B2C53AC301F8FA981C1BDB9D0%40phx.gbl.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1436858790.6948.YahooMailBasic%40web140905.mail.bf1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment