Re: [MW:23143] Welding of Had field steel

Main problem observed is start-stop point crack in specially SMAW. And PT is getting difficult to clear. Highly skilled welder is employed. So that possibility is ruled out of his ability and skill. Is this material prone to crack at start stop points only?

Hrushikesh H Sangamnerkar

On Jul 6, 2015 1:46 PM, "Srinivasan Jagannathan" <jsrisud@gmail.com> wrote:
Hi Hrushikesh,

What's the issue in welding Hadfield steel?

I will try to help you.

JS



On Sun, Jul 5, 2015 at 6:46 PM, Hrushikesh Sangamnerkar <hrushi612@gmail.com> wrote:

Hi..
Anyone has experience of welding Hadfield steel?

Hrushikesh H Sangamnerkar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2q1NBcWCZkdO1jxbHMjpcWCPvcnP4%2BKuizfX3HAgDkqkw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
J.SRINIVASAN

General Manager - Technical Services.

D&H SECHERON - INDORE

Mob: 7898989756

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKHQPVxMStKRirHgUeJ2VQqwmFnOTVGgS_UKbMVak_1_gG9Wzg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2o%3Dzo9z_cQoMmY92muVcrZFRnzChcVUg3tJHPbk2yqp7A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...