Dear all,

 In our district cooling CS ( ASTM A106 Gr,B) pipeline project, pipe wall thickness is from 3.2 mm to 20.62 mm.  and our WPS is qualified and now we have to conduct welder qualification test.So what is the minimum   test coupon  thickness we should select so that welder can weld upto 20.62 mm thickness pipe during production.

WPS Details:

Welding process: GTAW & SMAW

Base metal thickness range : 5 - 22 mm

Weld metal groove for GTAW ; 6mm and SMAW - 16 mm



Prince C Thomas

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0fdce533-3131-4418-bec0-6f0cef76fb24%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...