[MW:23212] Re: Ferrite Test Requirement on the Test Coupon

Copper block can be used for ferrite measurement . If you had been prepare standard chemical pad in controlled parameters ,can be analysised by WRC diagram .

Thanks
Vinay Tripathi
+919643886124(India)



On Thursday, July 23, 2015 at 1:39:00 PM UTC+5:30, Biplab Pal wrote:
Dear Experts.

We have a WPS for TP321 material tested 2005.
Client need additional Ferrite test on weld as per Client Std.
Can we use the previous test coupon for ferrite test or we can prepare a new coupon to do the additional Ferrite test.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/77bc209e-35ad-45cb-9353-4d916c5813a3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...