Friday, July 17, 2015

[MW:23171] Re: Economizer tube crack



在 2015年7月16日星期四 UTC+8下午2:28:52,Mian gee写道:
Dear All, please support to investigate the crack of ecanomozer tube.as
attached picture

    Type of tube- spirlly finned tube
     spiral material-sa-178a
     tube dia meter-219.1mm
      tube material-106b
       Maximum design pressure-5800kpa
     

Hi,

This photo don't provide enough information, first, confirm with some details.
1.you sure the leak point is cracking? or just like localized loss of thickness?
2 if localized loss of thickness, if other area have the same issue, or loss of thickness phenomena. if so, you should take care the corrosion issue, review the composition of the medium.
3.if leakage is due to crack, then you should distinguish crack the position where on the weld or along the HAZ, welding quality should be paid more attention. Also, excessive temperature in localized area is another potential reason.
In the end, I suggest more detailed investigation on other similary area is necessary action.
Thank you! 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e3235909-baa3-4def-8519-f61a21fbf634%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...