Wednesday, July 15, 2015

[MW:23168] Re: Whether we can weld SA 335 P11 and SA 335 P91

pl add a Gr22 piece in between . Welding between Gr 22 to Gr 91 shall be carried out  with Typ - B3 consumable with PWHT at 750-760 Deg C .

On Wednesday, June 17, 2015 at 7:29:47 PM UTC+5:30, arunkumar periasamy wrote:

In my condensing system my header line is having 2 materials

The line above sprayer which was connecting with condenser is SA 335 P11

And after sprayer till loop is SA 335 P91

 

Now my problem is whether we can weld or connect this SA 335 P11 and SA 335 P91 ?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f8111bf0-c910-4c2e-a4a4-d52328364b4e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...