Thursday, April 9, 2015

Re: [MW:23069] RT Report clarification / advise required

Dear Ismail,

please let us know whether you reviewed RT Report or RT film ? In
your quote RT report is mentioned only...

Shafad P.P
ASNT LEVEL 111 (RT,UT& MT)
India

On Wed, Apr 8, 2015 at 11:45 PM, Mohammed Ismail
<mohammedismail.inspections@gmail.com> wrote:
> Dear Experts,
>
>
>
> I am pleased to draw your attention and please provide your valuable input /
> advice / comment / clarification regarding my interpretation as below.
>
>
>
> The following is the requirement as referring to the attached 6600028289
> (OOK) schedule Q_quality requirements attachment 1 clause 2.2.1.
>
>
> Quote starts
>
>
> " When performing, reviewing or ensuring Nondestructive Testing in VT, MT,
> PT, RT or UT, he shall be certified in the specific method(s). When
> performing, reviewing or ensuring Radiographic Testing Film Interpretation
> (), Inspector shall be certified in ASNT Level II."
>
>
> Quote Ends
>
>
>
> My interpretation is RT report shall be reviewed or ensured by the inspector
> with ASNT Level II certified in RTFI.
>
> And after reviewing or ensuring the reports as per the requirements that
> report shall endorsed (singed) by that inspector who is qualified in RTFI .
>
>
> But the vendor is dis agreeing with the my statement.
>
>
>
> Please advise me.
>
>
> Thanks and best regards,
>
> Mohammed Ismail,
>
> Mechanical Inspector,
>
> vendor inspection department,
>
> Velosi.
>
> --
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at http://groups.google.com/group/materials-welding.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/CAF2Z%3DtU1K6RTNjHkkjN1ibYNxK3VNSufzza5j4BgLah%2Bx%2BYAJg%40mail.gmail.com.
> For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWuSzEttudxDmfd38WGKaKMXop%3DkpUTM-RFDMwVFJGqq255Rg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.