Are you certain it is the sockolet attached to an extended body gate valve?
your truly
H W JOSHI
ENGINEER MECHANICAL
TATA CONSULTING ENGINEERS LTD
MUMBAI - 400 083
TEL : 022 61148414
Kashif Syed <syedkashif.mech@gmail.com> Sent by: materials-welding@googlegroups.com 07-04-2015 16:37
|
|
Dear Members,
Good day.
I have a query regarding the partial fillet weld acceptance for Gate valve to sockelet connection from branch pipe.
We have welded the fillet weld of sockelet to Gate valve inlet but the client is not convinced with the weld joint strength and asking for technical acceptance of the pipe as per ASME B31.3. Attached drawing for reference.
The pressure is 7 bars.
Please comment whether there is any other option or this is acceptable with code reference.
--
Thanks & Regards,
Syed Kashif
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJeKOw28eJKvZO%2BtyH%2Bj-7_4o0LSrWUHHxgzs_mUKxcv-9D1ew%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.[attachment "sockolet.png" deleted by hemant w joshi/ME/MC-Nuclear/TCE]
----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF0D4885AB.F6E97364-ON65257E20.00413A53-65257E20.0040EE22%40tce.co.in.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment