[MW:23049] Acceptance of fillet partial weld

Dear Members,

Good day.

I have a query regarding the partial fillet weld acceptance for Gate valve to sockelet connection from branch pipe.

We have welded the fillet weld of sockelet to Gate valve inlet but the client is not convinced with the weld joint strength and asking for technical acceptance of the pipe as per ASME B31.3. Attached drawing for reference.

The pressure is 7 bars.

Please comment whether there is any other option or this is acceptable with code reference.



--
Thanks & Regards,


Syed Kashif 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJeKOw28eJKvZO%2BtyH%2Bj-7_4o0LSrWUHHxgzs_mUKxcv-9D1ew%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...