Re: [MW:23043] Maximum allowable temperature for HDPE

also depends on fluid. refer Shell DEP 30.10.02.13, check the catalog attached for reference

BR


On 5 April 2015 at 12:54, Himan Nikdin <himan.nikdin@outlook.com> wrote:
Thanks for your quick reply, would you please let me know related reference?


From: raghurambathula@gmail.com
Date: Sun, 5 Apr 2015 12:41:06 +0400
Subject: Re: [MW:23041] Maximum allowable temperature for HDPE
To: materials-welding@googlegroups.com

60 dec c
On 5 April 2015 at 12:26, Himan Nikdin <himan.nikdin@outlook.com> wrote:
Dear Experts

I need a reference to determine/specify Maximum allowable temperature to use HDPE material.

Regards,
Himan Nikdin 


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3Dy0EA10nJ4pBTAuzM-KD-oTNGw2uhhxfz7yyrhg2ZVFA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...