RE: [MW:23034] Raw material certificate


i think that you must be compared the physical and chemical propertys, and the  equivalent carbon.
Atte.
E carrion

Date: Wed, 1 Apr 2015 21:53:19 -0700
From: er.qaqc@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:23031] Raw material certificate

Dear experts,

while reviewing the material test certificates, I came across RAW material TC which is dated years back from the date of inspection of pipes which was ASTM A 105. and the RAW material TC does not shows A105 grade. its showing some other number. Pls clarify how I can make sure that it is the appropriate RAW material which is used for the manufacture of this pipe

Regards



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f39d79a8-443c-437a-8d72-5968d0526321%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...