[MW:23036] Real welding inspection Q&A you may or may not find a academic answer only on CSWIP 3.1 or CWI....(Continue...)


- Which things will you notice when review fim? first & second?
- how to check and count IQI on film? how many wire is OK? how length is acceptable?
- how is density? density range? ( my A: 2.0 - 4.0~4.5 or 2.0 to 1.8 - 4.0~4.5 or 2.0)
- what is "contrast"?
- Which is better? hight density or low density?
- How to calculate "Sensitivity".
- what is "definition"?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/149be1e3-5783-48cf-903a-29c037515ee2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...