Thursday, April 9, 2015

[MW:23067] Re: Crack in Duplex S.S material



Dear Abhishek,

Maybe you should check the whole welding process whether is corrdance with WPS . And you can do some basic test for the failure part, such as ferrite content.
To confirm root cause, then identify which welding process generate impact.

Thanks
Leon 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0969469b-fb7a-45b0-ab1d-515fbcad38c7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...