Re: [MW:21498] Does SS410S Weld overlay / butt welds (of SS 410S) requires PWHT?

Dear,

1.As per Sec ix 2013 table Qw/Qb 422 A/SA-240 Type 410s is P7 Gr-1 Uns no 41008 and if you go to ASME sec VIII div 1 3024 table UHA 32-2 P7 material required heat treatment. Holding temp 730 degree C. Upto 2 inch 1 hr/inch, 15 min minimum. More than 2 inch ,2 hr plus additional 15 min for every inch up to 5 inch.

If design code other than sec viii details may vary.

2.It depends on what Wps you are using as per welding code. PWHT is Essential veriable in most of the Wps  for CRO in Article 2 as per sec ix.

Regards
Shridev
On 31 Jul 2014 07:20, "S.Mohammed" <mohd52100@gmail.com> wrote:
>
> its depend whethet CRO done for strength purppse or corosion purpose.
> for strength req
> for corrosion not req.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...