Dear all,
I make WPS for P5B to P5B material 50 mm thk MDMT 18 deg. Celsius. , PWHT yes. No impact required then we done 2 Tensile & 4 side bend test. But at the time of laboratory test tensile pass but out of 4 side bend specimen 1 specimen was fail found 4 mm open discontinuity center of weld.
My question is can I do re side bend test from balance piece or new test piece to be weld.
Regards. ...
--To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment