 Hi everybody!
I have two PQR:
PQR 1: GTAW+ SMAW impact test at -28 degree Celsius ( SMAW use E7018); SMAW with back gouging.
PQR 2 SMAW+ SAW  impact test at -46 degree Celsius  ( SMAW use E7016-G); SMAW with back gouging.
Can I combine two PQR to make a WPS that SMAW+SAW (SMAW use E7018) and SMAW with gouging?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...