Dear Raghuram,
Actually, thé joint welded by m'y team passed thé RT. However, the RT report still mentionning "pitting in pipe's base métal", then cutting is not preferred.
My question is, Could this pitting comes from otherwise than base métal defect?
Many thanks
Sent from my ThinkPad S230u
Further exend the NDT and see the pitting (or any discontinuity) is in the base material or only HAZ area. You can even cut pipe little away and see inside.
On May 3, 2014 7:59 PM, "Lassaad" <lassaad.mokrani@gmail.com> wrote:--Dear Experts,
While radiographying a piping joint, our RT subcontractor has found some pitting indication in pipe base métal. Thé pipés are supplied by our end client. Our client tried to minimize thé issue saying" it might be caused by some operation done by us, being in HAZ limits".
Design code is B31.3
My question is what Could be the major reason of that defect? Is It most likely to be from piping base metal fabrication?
Please share your experience in this field.
Many thanks
Sent from my ThinkPad S230u
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment