Depending on magnitude of damage may have to grind to sound metal, PT , perform weld build up and machine to 125-250 aarh. Good luck

Sent from my iPhone

On Nov 2, 2013, at 4:03 AM, "N.Pandiyan" <asn.pandiyan@gmail.com> wrote:

6" # 150 FF Flange, ASME B16.5 flange face got corrosion and damage, how to repair at location? any portable tools & equipment available for re-machining and serration making? the gasket type is synthetic fibre.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone