[MW:19145] CORTEN A steel Welding for chimney flue liners

Hi,

I would request any support for preparing a WPS and WPQ. We will be using CORTEN A steel (A242/A588) for our steel flue liners (Chimney) and since we are doing the fabrication for the first time, we do not know the best procedure and materials for welding the liner cans...we are bringing CORTEN A steel rolls (8mm) and have purchased the roller welding equipment as well.

Can someone help me with this.

PS. I am new to the field. I have just completed my B.E Mech studies and joined this company. This would help me make a mark in the firm, if all goes well!! :)

Thanks in advance....

Sreeram Menon

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...