[MW:18456] Re: May E8018-C1 substitue E8018-G to weld Corten Steel

Hi everyone. i am also facing the almost same issue. we are short for E 8018 W2 electrode for corten steel. now contractor wanted to use  E 8018 G electrode as a W2 replacement. kindly guide me whether to allow him or not? reply kindly?

On Thursday, 20 October 2011 14:16:58 UTC+5, Tunisian Quality Engineer wrote:

Hi all

For welding Corten steel, we have in storage E8018-C1 Electrod, may it substitue  E8018-G, how can confirm ?

Regards
--
زكرياء غراب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...