Hi Rajasekhar,
Please see the draft from IS-2062, with explanations on IS-2062 E 350 Cu. The purpose of "copper addition" is to improve the weathering or resistance to atmospheric corrosion. Copper forms a self adhesive layer of "Reddish oxide" which protects the rest of the material from corrosion (see the attached picture).
See the attached documents for your reference.
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of RAJA SEKAR
Sent: Friday, August 02, 2013 7:01 AM
To: materials-welding@googlegroups.com
Subject: [MW:18330] Copper bearing steel
Please tell me the role of copper in steel(especially copper bearing steel like IS2062 E350 Cu)
Regards
Rajasekar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments