Friday, August 2, 2013

[MW:18331] Re: preheat requirement for alloy steel

Dear Sir,

Alloy steel has phase transformation while heating or cooling, so it require heat tratement. But for SS(P8 group only) it has no phase transformation, so it does not require any heat treatment.

If welding alloy steel with SS(P8) preheat is done on alloy steel side only as per the requirement.

Regards
Rajasekar

On Thursday, August 1, 2013 11:07:47 PM UTC+5:30, g.venkatesan06 wrote:
Dear experts

why preheat is mandatory for alloy steel and not mandatory for
stainless steel. Give some metallurgical reason and code reference.

Is joining alloy with stainless steel what is the preheat requirement.

Regards
venkatguru

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...